Thermal Conductivity: 130 W/mK
Tensile Strength: 83,000 Psi
Shear Strength: 48,000 Psi
Yield Strength: 73,000 Psi
Application: Aerospace, Defense, Shafts, Gears
Thermal Conductivity: 130 W/mK
Chemical Composition: 6%-8% Zinc
Fatigue Strength: Good
Application: Aerospace, Defense, Shafts, Gears
Temper: T6
Elongation: 11%
Electrical Conductivity: 33% IACS
Electrical Conductivity: 33% IACS
Melting Point: 477-635°C
Categories: Aerospace, Aluminum, Defense, Round Bar.
Chemical Composition: 6%-8% Zinc